The FTIR test results show mylar plastic sample is a polybutylene terephthalate polymer. Laraska 1, laraska 2 and laraska 3 plastic samples are polyvinyl alcohol polymers. Mika Asahi and Astralon Restorasi 1 plastic samples are polyvinyl chloride polymers. The plastic samples of Astralon Restorasi 2, Astralon Restorasi 3 and Plastik Sablon are poly (cyclohexadimethylene) terephthalate polymer. 3M double-sided tape samples are Cellulose Acetate-Based Backing Tapes and Acrylic Based Adhesive Tapes, kenko, joyco and subaru double-sided tape samples are Polypropylene-Based Backing Tapes and Rubber (Synthetic) Based Adhesive Tapes. There was an increase in MD direction tear strength values after aging in Mylar (50.67%), Plastik Sablon (11.58%), Mika Asahi (21.12%), Astralon Restorasi 1 (24.02), and Astralon Restorasi 3 (34.87%) samples and a decrease in Astralon Restoration 2 (3.27%) samples. There was an increase in tear strength values in the CD direction for Mylar (20.67%), Mika Asahi (15.14%), Astralon Restorasi 1 (30.26%), Astralon Restorasi 2 (27.01%) and Astralon Restorasi 3 (4.37%) and a decrease for Plastik Sablon samples (32.59%). There was an increase in tensile strength values after aging in Mylar (4.30%), Plastik Sablon (10.43%), Mika Asahi (5.42%) and Astralon Restorasi 3 (1.67%) samples and a decrease in Astralon Restorasi 1 (2.39%) and Astralon Restorasi 2 (5.84%) samples. GC-MS testing on all double-sided tape samples obtained the most dominant content results are Oxirane, 2-ethyl-2-methyl-, Cyclopentane, methyl- and 3-methylpentane.

References

Anwar Ul-Hamid., Khaled Y. Soufi., Luai M. Al Hadhrami., and Ahsan M. Shemsi, Failure investigation of an underground low voltage XLPE insulated cable, J. Anti-Corrosion Methods, and Materials 62(5):281-287, 2015.

Cheng Feng. Yi., Hui Zhao., Tong Hui Hao., Guo Hua Hu., Tao Jiang., and Qun Chao Zhang, Effect of poly (cyclohexanedimethylene terephthalate) on Microstructures, crystallization behaviour and properties of the poly (ester ether) elastomer, Materials 10, 2017.

Gorassini. A., Gianpiero A., Paolo. C., Alessandro. G, ATR-FTIR characterization of old pressure sensitive adhesive tapes in historic papers, Journal of Culture Heritage, 2016.

Horie. V, Materials for Conservation: Organic Consolidants, Adhesive and Coatings, 2nd ed, Elsevier Science, Butterworth-Heinemann, United Kingdom, 2010.

Irska. I., S. Paszkiewicz., K. Gorący., A. Linares., T.A. Ezquerra., R. Jędrzejewski., Z. Rosłaniec., and E. Piesowicz, Poly (butylene terephthalate)/ polylactic acid based copolyesters and blends: miscibility-structure-property relationship, eXPRESS Polymer Letter 14(1):26-47, 2020.

Krimm, S., C.Y. Liang and G.B.B.M. Sutherland, Infrared Spectra of High Polymers. V. Polyvinyl Alcohol, J. of Polymer Science 22:227-247, 1956.

McKeen. L.W, Film Properties of Plastics and Elastomers, 4th ed, Elsevier Science, William Andrew, United Kingdom, 2017.

Munro. S.N, Polyester Encapsulation, J. Conserve O Gram 13/3, Virginia, 1993.

Downloads

Published

2023-11-15

How to Cite

Payanti, T. D., Sofiati, D. A. ., & Suryanah, Y. (2023). Paper-Based Archives Encapsulation: Identifying Physical-Mechanical and Chemical Materials. Jurnal Kearsipan, 18(2). https://doi.org/10.46836/jk.v18i2.272